| Name | PVC FILM | Order Number | --- |
| LOT. Number | SAMPLE | MFG Date | 2014/05/26 |
| Quantity | 5KG | EXP Date | 2015/05/25 |
| Structure | 210mm×300micron | Report Date | JF20140530 |
| Item | Specification | Test Result | Conclusion | |||
| Appearance | The PVC Sheet Should be Transparent, uniform. Disallow to have the wrinkledness, greasy dirt, eyewrinker, perforation, impurity. Fisheye's Diameter>1.3mm | Match the Norm | Qualified | |||
| Size | Width mm | ±2 | ---- | -- | ||
| ±1 | 210 | Qualified | ||||
| Thickness mm | ±0.02 | 0.29~0.31 | Qualified | |||
| Identify | Infrared spectrum analysis | Should be uniform to the antitheses spectrum | -- | -- | ||
| Density g/cm3 | 1.35~1.45 | 1.37 | Qualified | |||
| Physics |
Water Vapor Transmission g/m2·24h 23ºC,RH90% |
≤2.5 | 2.21 | Qualified | ||
| Oxygen Transmission cm3/m2·24h·0.1MPa |
≤30 | 18 | Qualified | |||
| Tensile Strength MPa | MD:≥ 44 | 52.1 | Qualified | |||
| TD:≥ 44 | 54.3 | Qualified | ||||
| Falling Ball Impact Brittle Rate | TD: no more than 2 damage | 0 | Qualified | |||
| MD: no more than 2 damage | 0 | Qualified | ||||
| Heating Shrinking rate % | -6~+6 | -3.2,+1.4 | Qualified | |||
| Heating Sealing Strength N/15mm | ≥7.0 | 13.6 | Qualified | |||
| The Content of VCM mg/kg | ≤1 | 0.4 | Qualified | |||
| Test of Extraction | Degree of Clear | Ought to clear | Clear | Qualified | ||
| Test of Oxidation | Difference of Titer≤1.0 ml | 0.78 | Qualified | |||
| Heavy Metal mg/kg | ≤1 | <1 | Qualified | |||
| Non-Volatile | water mg | ≤30.0 | 10 | Qualified | ||
| 65%Ethanolmg | ≤30.0 | 6.8 | Qualified | |||
| Hexanemg | ≤30.0 | 2.7 | Qualified | |||
| Barium | Ought to clear | Match the Norm | Qualified | |||
| Plasticizer | Less than 6% | 2% | Qualified | |||